High Tenacity Polyester Yarn
Large bright, semi-dull polyester FDY: fineness 200D-600D, breaking strength 4.0cN/dtex. Can be customized according to customer requirements.
Category:
Keywords: Industrial filament / FDY
Contact Us
Lu Chongguo +86-13506296398
Lu Jing +86-13016780108
Mail: sales@zxxy.com.cn
Product Description
High Tenacity Polyester Yarn Specifications
|
Yarn specifications |
77dtex/24f |
110dtex/36f |
167dtex/48f |
233dtex/72f |
278dtex/72F |
466dtex/144f |
555dtex/144f |
|
|
70D/36f |
100D/36f |
150D/48f |
210D/72f |
250D/72f |
420D/144f |
500D/144f |
||
|
Product mark |
ZX-P77HT |
ZX-P110HT |
ZX-P167HT |
ZX-P233HT |
ZX-P278HT |
ZX-P466HT |
ZX-P555HT |
|
|
1 |
Linear density (dtex) |
77±1.54 |
110±2.2 |
167±3.34 |
233±4.7 |
278±5.6 |
466±9.32 |
555±11.2 |
|
2 |
Breaking Force (N) |
≥4.7 |
≥7.84 |
≥11.76 |
≥16.46 |
≥19.6 |
≥32.9 |
≥39.2 |
|
3 |
Breaking tenacity(g/D) |
≥7.8 |
≥8.0 |
≥8.0 |
≥8.0 |
≥8.0 |
≥8.0 |
≥8.0 |
|
4 |
Hot air shrinkage (%) |
5±1.2 |
5±1.2 |
5±1.0 |
5±1.0 |
5±1.0 |
5.0±1.0 |
5.0±1.0 |
|
5 |
Elongation at break(%) |
16.0±3.0 |
||||||
|
6 |
CV of LD (%) |
≤2.0 |
||||||
|
7 |
CV of BF (%) |
≤5.0 |
||||||
|
8 |
CV of EAB (%) |
≤8.0 |
||||||
|
9 |
Dye uniformity (Gray card) |
4-6 |
||||||
|
10 |
Whiteness |
≥80 |
||||||
|
11 |
Bobbin weight (kg,incl.tube) |
8.0±0.1(full cylinder) 3.5-5.5(Small tube) |
12±0.1(Full cylinder) 3-7(Trochlet) |
|||||
|
12 |
Bobbin size (mm) |
Ф150×110 |
Ф150*110 |
|||||
|
Note: The national standard method is used for testing, and the dry heat shrinkage rate (%)(177℃×2min,0.05g/D) |
||||||||
|
Yarn specifications |
924dtex/192f |
1100dtex |
1670dtex/432f |
|
|
|
|
|
|
840D/192f |
1000D/192f |
1500D/432f |
|
|
|
|
||
|
Product mark |
ZX-P924HT |
ZX-P1100HT |
ZX-P1670HT |
|
|
|
|
|
|
1 |
Linear density (dtex) |
924±30 |
1100±30 |
1670±30 |
|
|
|
|
|
2 |
Breaking Force (N) |
≥65.80 |
78.4 |
≥117.6 |
|
|
|
|
|
3 |
Breaking tenacity(g/D) |
≥8.0 |
≥8.0 |
≥8.0 |
|
|
|
|
|
4 |
Hot air shrinkage (%) |
5±1.2 |
5±1.2 |
5±1.0 |
|
|
|
|
|
5 |
Elongation at break(%) |
16.0±3.0 |
||||||
|
6 |
CV of LD (%) |
≤2.0 |
||||||
|
7 |
CV of BF (%) |
≤5.0 |
||||||
|
8 |
CV of EAB (%) |
≤8.0 |
||||||
|
9 |
Dye uniformity (Gray card) |
4-6 |
||||||
|
10 |
Whiteness |
≥80 |
||||||
|
11 |
Bobbin weight (kg,incl.tube) |
12±0.1(Full cylinder)3.5-8.5(Small tube) |
||||||
|
12 |
Bobbin size (mm) |
Ф300×110 |
||||||
|
Note: The national standard method is used for testing, and the dry heat shrinkage rate (%)(177℃×2min,0.05g/D) |
||||||||
Related Products
Feedback